HOME > Article > DetailStrength Retention in Hot-Pressed Si3N4 Ceramics with Lu2O3 Additives after Oxidation Exposure in Air at 1500C(Lu2O3を添加したホットプレスSi3N4の1500℃酸化後の強度変化)Shuqi Guo, Naoto Hirosaki, Yoshinobu Yamamoto, Toshiyuki Nishimura, Mamoru Mitomo. Journal of the American Ceramic Society 85 [6] 1607-1609. 2002.https://doi.org/10.1111/j.1151-2916.2002.tb00319.x NIMS author(s)GUO, ShuqiHIROSAKI, NaotoNISHIMURA, ToshiyukiFulltext and dataset(s) on Materials Data Repository (MDR)Created at: 2016-05-24 11:49:04 +0900 Updated at: 2026-10-08 08:02:16 +0900