HOME > Presentation > DetailHCM12A鋼溶接継手のクリープ破断寿命評価(Creep life assessment of HCM12A steel weldment)田淵 正明. 高温材料強度部門委員会 非弾性解析WG. 2004-05-14. InvitedNIMS author(s)TABUCHI, MasaakiFulltext and dataset(s) on Materials Data Repository (MDR)Created at: 2017-01-08 05:13:24 +0900Updated at: 2024-03-05 11:40:11 +0900