HOME > Article > DetailDiscontinuous Precipitation of σ Phase during Recrystallization in a Cold-rolled Fe-10%Cr-30%Mn Austenite.(冷間圧延したFe-10Cr-30Mnオーステナイト鋼における再結晶中の6相の不連続析出。)F. Abe, H. Araki, 野田哲二, T. Noda. Materials Science and Technology 4 [10] 885-893. 1988.https://doi.org/10.1179/mst.1988.4.10.885 NIMS author(s)ABE, FujioFulltext and dataset(s) on Materials Data Repository (MDR)Created at: 2016-05-24 11:22:54 +0900Updated at: 2024-05-02 06:36:17 +0900