HOME > Presentation > Detail(Precipitation during HPT deformation and subsequent ageing in Mg - 3.4 mol% Zn alloy)ロザリエ ジュリアン マーク, パウ ブライアン リチャード, 孟 凡強, 土谷 浩一. JIM Fall Meeting. 2014.NIMS author(s)TSUCHIYA, KoichiFulltext and dataset(s) on Materials Data Repository (MDR)Created at: 2017-01-08 04:51:55 +0900Updated at: 2017-07-10 21:55:53 +0900