最新データに基づく寿命評価式,許容引張応力および 長手継手の溶接継手強度低減係数
(A Life Assessment Formula, Allowable Stress Value, and a Welded Joint Strength Reduction Factor Based on the Newest Data)

橋本正徳, 木村 一弘, 屋口正次, 中井浩之.
火力原子力発電 1027-1031. 2012.